Zirconite

B.J.M. Laboratories Ltd. · source

Zirconite

Dual-cure permanent adhesive resin cement designed for Zirconia

  • Permanent cementation of Ceramic and Zirconia restorations
  • Proven Color Stability over time.

An innovative dual-cure permanent adhesive resin cement specially formulated for Zirconia cementation

  • ISO 4049 classification: Type 2, Class 3.
  • Self-etch, self-adhering, dual cured, radiopaque permanent resin cement that does not require etching, priming, or bonding.
  • Radiopacity value above 2.5 mm Aluminium. (Radiopacity is defined as the ability of a material to be visible in x-ray photographs.)
  • Chemical affinity for metal and Zirconia.
  • Dual-cure cement – it has a self curing mechanism which can also be light cured for an immediate set and extra strength at the margins.
  • Features high retention and total margin integrity.
  • Administration via Automix syringe saves application time and guarantees consistent mix.
  • Available in 3 shades: Dentin, Translucent, White, To see shade guide visit www.bjmlabs.com.
  • Marketed since 2009. No complaints of any health-related or chemical performance issues were received.

Technical Data

Compressive strength: > 150 MPa

Flexural strength: > 100 MPa

Water sorption: ≤ 40 μg/mm3

Solubility: ≤ 7.5 μg/mm3

Shear bond strength to etched enamel: > 10 MPa

Shear bond strength to un-etched dentin: > 5 MPa

Shear bond strength to pretreated metal alloy: > 10 MPa

Shear bond strength to un-treated ceramic surface (Zirconia): > 5 MPa

Film thickness: <50

Radiopacity: >100 % Al

Working time (in ambient light and temperature): > 90 seconds, in the 1.5 - 3.5 min interval

Setting time (in oral temperature): < 10 minutes, in the 2.5 - 4.5 min interval

Light curing time: 10 – 20 seconds

Compatible with LED: Yes

Compatible with halogen light: Yes

Compatible with plasma ark light lamp: Yes

Shelf life: 2 Years

Product Information

ManufacturerB.J.M. Laboratories Ltd.
Shelf Life2 Years
Solubility≤ 7.5 μg/mm3
ApplicationPermanent cementation of Ceramic and Zirconia restorations
Curing TypeDual-cure
Radiopacity>100 % Al
Film Thickness<50
Water Sorption≤ 40 μg/mm3
Flexural strength> 100 MPa
Light Curing Time10 – 20 seconds
Compatible With LedYes
Compressive strength> 150 MPa
Iso 4049 ClassificationType 2, Class 3
Compatible With Halogen LightYes
Setting Time (in Oral Temperature)< 10 minutes, in the 2.5 - 4.5 min interval
Shear Bond Strength To Etched Enamel> 10 MPa
Compatible With Plasma Ark Light LampYes
Shear Bond Strength To Un Etched Dentin> 5 MPa
Shear Bond Strength To Pretreated Metal Alloy> 10 MPa
Working Time (in Ambient Light And Temperature)> 90 seconds, in the 1.5 - 3.5 min interval
Shear Bond Strength To Un Treated Ceramic Surface (zirconia)> 5 MPa