Cast UV 3.0 is developed for the production of high-precision dental casts. Its low viscosity and optimized cure depth help reduce print time, material consumption, and wash time. Printing results are precise and without any misshapes. The burnout process leaves no residue in the mold, which facilitates removable partial dentures (RPD), post and core, and crowns with metal casts. It also works for crowns with zirconia, veneers, and ceramic inlays.
Key Features
- Clean Burn-out
- Dimensional Stability
- Vivid Detail Restoration
- High-precision Casting
Basic Performance
| Properties | Unit | Standard | Result |
|---|---|---|---|
| Flexural Strength | MPa | ASTM D790 | 72.3-84.5 |
| Insertion Temperature | ℃ | / | 900-950 |
| Holding Time | Hour | / | 1-1.5 |
| Wall Thickness | mm | / | ≥0.35 |
| Storage Time | Hour | / | <10 |
| Ash Value | / | / | <0.03% |
Application
- Crown (metal/ceramic casting)
- Veneer (ceramic casting)
- Inlay (ceramic casting)
Informations produit
| Fabricant | HeyGears GmbH |
|---|---|
| Couleur | Red, Clear |
| Ash Value | <0.03% |
| Holding Time | 1-1.5 Hour |
| Storage Time | <10 Hour |
| Certification | FDA, NMPA, CE |
| Specification | 1000 g/Bottle |
| Wall Thickness | ≥0.35 mm |
| Résistance à la flexion | 72.3-84.5 MPa (ASTM D790) |
| Insertion Temperature | 900-950 ℃ |
| Machine Compatibility | A2D, A2D 4K, ChairSide Pro, A3D |